Learn · Woodworking basics
How to glue and clamp wood
A good glue joint is stronger than the wood around it. Getting one takes the right glue, parts that fit, and a glue-up you’ve rehearsed before the bottle comes out.
Choose a glue
| Glue | Use it for | Good to know |
|---|---|---|
| Yellow wood glue (PVA), such as Titebond Original | Most indoor furniture and cabinets | Easy to spread, and cleans up with water. Not for outdoor use. |
| Water-resistant and waterproof PVA, such as Titebond II and III | Outdoor furniture, planters, cutting boards | Titebond III gives you longer to work, and can be used in a cooler shop. |
| Polyurethane glue | Outdoor projects, oily woods, wood to other materials | Waterproof. It foams as it cures, so clamp well, and wear gloves. |
| Epoxy | Gaps, repairs, wood to metal or stone | Two parts mixed together. It fills gaps, which most wood glues don’t. |
| CA glue (super glue) | Small repairs, holding parts while other glue dries | Sets in seconds, but is too brittle for joints that carry a load. |
Know how long you have
- Open time is how long you have from spreading the glue to closing the joint. Titebond Original gives you 4 to 6 minutes, and Titebond III 8 to 10, at 70°F. A warm, dry shop shortens it.
- Clamp time is how long the joint stays clamped: about 30 minutes for these glues.
- Full strength takes much longer. Leave the joint alone for a day before you stress it, plane it or cut it.
- Temperature: Titebond Original needs the room, the glue and the wood above 50°F; Titebond III works down to 47°F.
Check the bottle for your glue’s own times and temperatures.
Make a good glue joint
- The parts should fit without forcing and without gaps. Clamps should close a joint, not bend parts to make it close. Most wood glues don’t fill gaps.
- Glue long grain to long grain. End grain soaks up glue and holds poorly. See Wood joints for beginners.
- Glue fresh, clean surfaces. Freshly cut or planed wood bonds best.
- Use enough glue. Once the joint is clamped, you want a thin, even bead squeezing out along it. No squeeze-out means too little glue; glue running down the boards means too much.
- Use firm, even pressure. Tighten until the joint closes and glue squeezes out along its whole length. Add a clamp wherever there’s no squeeze-out. Cranking the clamps as hard as you can doesn’t help.
Do a dry run first
Before any glue goes on, put the whole thing together with clamps, in the order you’ll do it for real. Open every clamp to about the right size, and keep them within reach. Know how you’ll check that it’s square: measure both diagonals of a box or frame, which are equal when it’s square. It’s far better to find a problem now than with the glue setting.
Glue up a panel
To make a wide top from narrower boards:
- Make sure the edges are straight, so they meet along their whole length with no gaps.
- Lay the boards out for the best look, and draw a big V across them so you can put them back in order.
- Spread glue on the edges, then clamp, alternating clamps above and below the panel so it stays flat.
- Keep the faces flush as you tighten. A straight board clamped across each end (a caul) helps.
- Leave it clamped for the clamp time, then let the glue cure before you flatten the panel.
Clean up squeeze-out
Dried glue blocks stain and finish, leaving pale patches. Let the squeeze-out set until it’s rubbery, about 20 minutes, then lift it off with a scraper or chisel. Or wipe it off straight away with a damp rag, taking care not to smear it into the grain. Masking tape along the joint before you glue catches it too.